The waste rubber tires are affected by many factors during the pyrolysis and refining process, including temperature, heating rate, pyrolysis time, pressure and the properties of the waste rubber itself. These factors always affect the pyrolysis performance and pyrolysis products.
The influence of temperature on the cracking of waste rubber is crucial. It not only affects the cracking process, but also affects the proportion of cracking products. When the temperature is lower, it can reduce the secondary reaction of macromolecular organic matter, generate more molecular chains above C5, and have more oil content. As the temperature continues to rise, while macromolecules continue to crack, small molecules also undergo secondary polymerization reactions, resulting in an increase in olefin gas, a decrease in the amount of oil produced, and an increase in flammable gas. Carbon black components and tar components gradually decrease as the temperature increases.
The temperature rise rate is one of the important parameters that affects the cracking of waste rubber. The impact of the temperature rise rate on the cracking of waste rubber is mainly reflected in the proportion of cracking products and productivity. The main reason for this effect is that the increase in temperature rise rate directly affects the mass transfer rate of the cracked products. Generally speaking, when the temperature rise rate is high, the pyrolysis time of waste rubber is short, the proportion of gas in the pyrolysis products is larger, and the proportion of solid carbon black and oil is smaller. When the temperature rise rate is low, the cracking time of waste rubber is long, and the organic matter that has just begun to crack will combine with each other to form a stable solid, and the solid yield increase rate is increased.
Cracking time refers to the reaction residence time of waste rubber in the cracking chamber. The pyrolysis time will also affect the proportion of each component of the pyrolysis product. The large size of the waste rubber requires a long pyrolysis time. The longer the pyrolysis time means the longer the residence time in the pyrolysis chamber and the more complete the pyrolysis reaction. However, The pyrolysis efficiency is low, and secondly, the longer residence time in the pyrolysis chamber will increase secondary reactions, which is not conducive to improving the quality of the pyrolysis products.
The properties of waste rubber are mainly reflected in the outer dimensions of waste rubber. If the size of the waste rubber is small, the heating area during the cracking process will be large, the heat transfer speed will be fast, the cracking reaction rate will increase, and the cracking will be uniform. If the size of the waste rubber is large, the heat transfer rate is low, and the cracking time is long, the secondary cracking reaction is likely to increase, and the cracking effect is poor. Therefore, in order to obtain better pyrolysis products, waste rubber is usually crushed to obtain rubber powder.

The pyrolysis oil produced by the waste tire pyrolysis machine can be widely used as industrial fuel. If the waste oil is further refined into diesel or gasoline through a waste oil distiller, it can be used in low-speed engines such as excavators, road rollers or loaders, thus helping to alleviate the energy crisis.